CM-30 series pvc stabilizer can solve poor flowability of PVC plastic and wood melt, poor plastic-wood bonding and difficult processing.
It has excellent thermal stability, lubricity and weather resistance, initial coloring, long times extruding and mechanical failures, extend the extruder life of 3-5 years.
Package: 25kg per bag by plastic weaved bag.
Usage: WPC Wall Panel, WPC Floor, etc.
Online Service
+86-318-2100354Item | Unit | CM-300 | CM-305 |
Appearance | White or yellowish flake | ||
PbO content, | % | 29% ± 1.0 | 23% ± 1.0 |
Initial melting point, ℃, | ≥ | 55 | 55 |
Heating Loss, % | ≤ | 1.0 | 1.0 |
Recommend Dosage | 4.0 - 6.0kg per 100kg PVC Resin |
WPC Floor | WPC Door Panel |
WPC/PVC Wall Panel | WPC Wall Panel |
Design the most suitable Formula
Give the Lowest Formula cost
Improve the product quality
Regular Time follow produce and technical support
According to the SGS test, it meets the RoHS 2.0 standard.